Chemical Composition
0.12
%  (maximum)  
17 to 19
%    
1.8 to 2.3
%    
51.7 to 61.7
%    (estimate)
2
%  (maximum)  
2.5 to 3.5
%    
17 to 19
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
1.5
%  (maximum)  
0.8
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
200
MPa    
20
% strain    
160 to 230
   
 
Other Information