Chemical Composition
0.25 to 0.35
%    
97.1 to 98.1
%    (estimate)
1.1 to 1.4
%    
0.3
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.6 to 0.8
%    
 