Chemical Composition
0.57 to 0.65
%    
97.6 to 98.4
%    (estimate)
0.7 to 1.1
%    
0.06
%  (maximum)  
0.15 to 0.25
%    
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
570
MPa    
830 to 980
MPa    
7
% strain    
 