Chemical Composition
0.2
%  (maximum)  
97.7 to 99.9
%    (estimate)
1.5
%  (maximum)  
0.05
%  (maximum)  
0.05
%  (maximum)  
0.1 to 0.55
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
350
MPa    
490 to 630
MPa    
22
% strain    
 
Other Information