Chemical Composition
0.33
%  (maximum)  
98.3 to 99.2
%    (estimate)
0.85 to 1.2
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
255
MPa  (minimum)  
505 to 640
MPa    
22
% strain  (minimum)  
 
Other Information