Chemical Composition
0.12
%  (maximum)  
0.5 to 1.25
%    
0.25 to 0.55
%    
96 to 98.7
%    (estimate)
0.2 to 0.5
%    
0.65
%  (maximum)  
0.07 to 0.15
%    
0.035
%  (maximum)  
0.25 to 0.75
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
335
MPa    
510 to 610
MPa    
22
% strain    
 