Chemical Composition
0.08
%  (maximum)  
17 to 20
%    
0.75
%  (maximum)  
61.2 to 74
%    (estimate)
2
%  (maximum)  
0.75
%  (maximum)  
1.1
%  (maximum)  
9 to 13
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
724 to 965
MPa    
20
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®