Chemical Composition
0.015 to 0.12
%    
0.2
%  (maximum)  
0.25
%  (maximum)  
96.7 to 99.8
%    (estimate)
1.5
%  (maximum)  
0.1
%  (maximum)  
0.01 to 0.06
%    
0.3
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.5
%    
0.02 to 0.06
%    
0.02 to 0.1
%    
0.01 to 0.06
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
335
MPa    
490 to 610
MPa    
23
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data