Chemical Composition
0.39 to 0.46
%    
97.4 to 98.3
%    (estimate)
1.3 to 1.65
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
480
MPa  (minimum)  
750 to 1050
MPa    
12
% strain  (minimum)  
 
Other Information