Chemical Composition
0.37 to 0.43
%    
0.65 to 0.95
%    
95 to 96.5
%    (estimate)
0.55 to 0.85
%    
0.15 to 0.3
%    
1.6 to 2
%    
0.035
%    
0.035
%    
0.15 to 0.4
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®