Chemical Composition
0.32 to 0.42
%    
1.2 to 1.5
%    
0.3
%  (maximum)  
92.6 to 94.6
%    (estimate)
0.25 to 0.5
%    
0.35 to 0.45
%    
3 to 3.5
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.17 to 0.37
%    
0.1 to 0.25
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
785
MPa  (minimum)  
900
MPa  (minimum)  
13
% strain  (minimum)  
 