Chemical Composition
0.18
%  (maximum)  
0.25
%  (maximum)  
97.6 to 99.9
%    (estimate)
1
%  (maximum)  
0.1
%  (maximum)  
0.3
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.15 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
215
MPa    
360 to 460
MPa    
26
% strain    
 