Chemical Composition
0.3 to 0.38
%    
1.3 to 1.7
%    
94.7 to 96.5
%    (estimate)
0.5 to 0.8
%    
0.15 to 0.3
%    
1.3 to 1.7
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
800
MPa  (minimum)  
1000 to 1300
MPa    
10
% strain  (minimum)  
 
Other Information
Links