Chemical Composition
0.8 to 1.2
%    
0.3 to 0.37
%    
1 to 1.3
%    
95.5 to 97.3
%    (estimate)
0.5 to 0.8
%    
0.15 to 0.25
%    
0.03
%  (maximum)  
0.035
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
600
MPa  (minimum)  
800 to 1000
MPa    
14
% strain  (minimum)  
248
 (maximum)  
 