Range attributes
0.8 to 1.2
%    
248
 (maximum)  
0.3 to 0.37
%    
1 to 1.3
%    
14
% strain  (minimum)  
95.5 to 97.3
%    (estimate)
0.5 to 0.8
%    
0.15 to 0.25
%    
0.03
%  (maximum)  
0.035
%  (maximum)  
0.5
%  (maximum)  
800 to 1000
MPa    
600
MPa  (minimum)  
 
Discrete attributes
Short text attributes
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
International
Wrought nitriding steel blooms, billets and slabs; QT, ann hardness, d<70 mm.
33CrAlMo5-4
ISO 683-10
 
Long text attributes
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Wrought nitriding steel blooms, billets and slabs; QT, ann hardness, d<70 mm.
 
Hyperlink attributes
Integer attributes
Further Information



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®