Chemical Composition
0.28 to 0.35
%    
2.7 to 3.2
%    
91.8 to 93.8
%    (estimate)
0.15 to 0.45
%    
2.6 to 3
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.1 to 0.4
%    
0.4 to 0.7
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1670
MPa    
 
Other Information