Chemical Composition
0.0008 to 0.005
%    
0.27 to 0.33
%    
0.15 to 0.25
%    
97.3 to 98.4
%    (estimate)
1.1 to 1.4
%    
0.1
%  (maximum)  
0.2
%  (maximum)  
0.025
%  (maximum)  
0.02
%  (maximum)  
0.1 to 0.4
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
450
MPa    
14
% strain    
 
Other Information