Chemical Composition
0.27 to 0.33
%    
0.6 to 0.9
%    
0.2
%  (maximum)  
94.3 to 95.9
%    (estimate)
0.3 to 0.6
%    
0.1
%  (maximum)  
2.75 to 3.15
%    
0.02
%  (maximum)  
0.02
%  (maximum)  
0.17 to 0.37
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
785
MPa  (minimum)  
980
MPa  (minimum)  
9
% strain  (minimum)  
 
Other Information
Links