Chemical Composition
0.32 to 0.39
%    
97.8 to 98.2
%    (estimate)
1.35 to 1.65
%    
0.04
%    
0.08 to 0.13
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties