Chemical Composition
0.015 to 0.06
%    
0.16
%  (maximum)  
0.3
%  (maximum)  
0.25
%  (maximum)  
96.1 to 100
%    (estimate)
1.8
%  (maximum)  
0.1
%  (maximum)  
0.012
%  (maximum)  
0.06
%  (maximum)  
0.3
%  (maximum)  
0.25
%  (maximum)  
0.02
%  (maximum)  
0.45
%  (maximum)  
0.06
%  (maximum)  
0.1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 