Chemical Composition
0.15
%  (maximum)  
0.4 to 0.8
%    
0.25 to 0.55
%    
95.5 to 98.8
%    (estimate)
0.5 to 1.5
%    
0.65
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.5
%  (maximum)  
0.02 to 0.12
%    
0.15
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
345
MPa    
510 to 610
MPa    
22
% strain    
 