Chemical Composition
0.08 to 0.15
%    
4 to 6
%    
92 to 94.9
%    (estimate)
0.3 to 0.6
%    
0.45 to 0.65
%    
0.025
%  (maximum)  
0.02
%  (maximum)  
0.3 to 0.6
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
390
MPa    
590 to 740
MPa    
17
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data