Chemical Composition
0.2 to 0.5
%    
0.03 to 0.08
%    
0.5
%  (maximum)  
19 to 22
%    
0.5
%  (maximum)  
41.1 to 50.6
%    (estimate)
1.5
%  (maximum)  
0.03
%  (maximum)  
0.1
%  (maximum)  
30 to 32.5
%    
0.015
%  (maximum)  
0.01
%  (maximum)  
0.7
%  (maximum)  
0.2 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
170
MPa    
500 to 750
MPa    
35
% strain    
 
Other Information