Chemical Composition
0.48 to 0.58
%    
20 to 22
%    
62.1 to 67.9
%    (estimate)
8 to 10
%    
0.35 to 0.5
%    
3.25 to 4.5
%    
0.05
%  (maximum)  
0.03
%  (maximum)  
0.25
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
580
MPa    
950 to 1200
MPa    
8
% strain    
 