Chemical Composition
0.3 to 0.5
%    
24 to 26
%    
33.4 to 40.7
%    (estimate)
1.5
%  (maximum)  
34 to 36
%    
0.035
%  (maximum)  
0.03
%  (maximum)  
1 to 2.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
230
MPa    
5
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®