Chemical Composition
0.2
%  (maximum)  
19 to 21
%    
61.1 to 68.5
%    (estimate)
2
%  (maximum)  
0.11
%  (maximum)  
11 to 13
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1.5 to 2.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
230
MPa    
500 to 750
MPa    
30
% strain    
 