Chemical Composition
0.07
%  (maximum)  
18 to 20
%    
61.4 to 71
%    (estimate)
1.5
%  (maximum)  
2 to 2.5
%    
1
%  (maximum)  
9 to 12
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
1.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
185
MPa    
440 to 640
MPa    
20
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data