Chemical Composition
0.03
%  (maximum)  
17.5 to 19.5
%    
57.3 to 66.5
%    (estimate)
2
%  (maximum)  
3 to 4
%    
0.11
%  (maximum)  
13 to 16
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
200
MPa    
500 to 700
MPa    
30 to 40
% strain    
 