Chemical Composition
0.05 to 0.15
%    
16 to 19
%    
66.4 to 78
%    (estimate)
2
%  (maximum)  
0.8
%  (maximum)  
0.11
%  (maximum)  
6 to 9.5
%    
0.045
%  (maximum)  
0.015
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
195
MPa    
500 to 750
MPa    
40
% strain    
 
Other Information