Chemical Composition
0.65 to 0.75
%    
14 to 16
%    
80.7 to 85
%    (estimate)
1
%  (maximum)  
0.4 to 0.8
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
0.7
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 