Chemical Composition
0.03
%  (maximum)  
20 to 21.5
%    
50.3 to 57.8
%    (estimate)
4 to 6
%    
3 to 3.5
%    
0.2 to 0.35
%    
0.25
%  (maximum)  
15 to 17
%    
0.025
%  (maximum)  
0.01
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
365
MPa    
740 to 930
MPa    
35
% strain    
 
Other Information