Chemical Composition
0.03
%  (maximum)  
16.5 to 18.5
%    
60.2 to 67.8
%    (estimate)
2
%  (maximum)  
2.5 to 3
%    
0.15 to 0.25
%    
13 to 15
%    
0.045
%  (maximum)  
0.015
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
295
MPa    
490 to 690
MPa    
30
% strain    
 
Other Information