Chemical Composition
0.57 to 0.65
%    
0.4
%  (maximum)  
97.1 to 98.8
%    (estimate)
0.6 to 0.9
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
520
MPa    
800 to 950
MPa    
13
% strain    
 
Other Information