Chemical Composition
0.42 to 0.5
%    
0.4
%  (maximum)  
97.3 to 99.1
%    (estimate)
0.5 to 0.8
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
430
MPa    
650 to 800
MPa    
16
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data