Chemical Composition
0.015
%  (minimum)  
0.16
%  (maximum)  
97.8 to 100
%    (estimate)
1.2
%  (maximum)  
0.09
%  (maximum)  
0.025
%  (maximum)  
0.02
%  (maximum)  
0.5
%  (maximum)  
0.15
%  (maximum)  
0.1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
260
MPa    
370 to 490
MPa    
30
% strain    
 
Other Information