Chemical Composition
0.1
%    
16 to 18
%    
73.9 to 77.9
%    (estimate)
6 to 8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276
MPa    
60
% strain    
 
Other Information
Annealed: 110,000 TS; 40,000 YS; 60 El; 85 HRB. For aircraft structural members, railroad cars, household utensils, diaphragms, springs. Type 301 stainless steel, austenitic, non-hardenable.
KRUPP-V2AFH
 
Links
Organizations

 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®