Chemical Composition
0.1
%  (maximum)  
16 to 18
%    
65.2 to 72.3
%    (estimate)
1.7 to 2.7
%    
10 to 14
%    
Nb=10xC
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
241 to 310
MPa    
586 to 655
MPa    
50 to 60
% strain    
150 to 190
   
 
Other Information
Annealed: 85,000-95,000 TS; 35,000-45,000 YS; 60-50 El; 75-60 RA; 150-190 HB; For acid resistant chemical plant equipment; Type 316 Cb; stainless, austenitic.
KRUPP V4 AE-TI
 