Chemical Composition
0.15
%    
18
%    
73.9
%    (estimate)
8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
538 to 696
MPa    
55 to 65
% strain    
140 to 175
   
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®