Chemical Composition
0.12
%    
19.5
%    
62.6
%    (estimate)
8
%    
9
%    
0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
310
MPa    
45
% strain    
 
Other Information
Links
Organizations

 



No warranty is given for the accuracy of these data