Chemical Composition
0.1
%  (maximum)  
20.5 to 21.5
%    
64.9 to 67.5
%    (estimate)
10.5 to 11.5
%    
1.5 to 2
%    
Approx. 0.17 N and 0.05 Ce
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
310
MPa    
650 to 850
MPa    
35
% strain    
 
Other Information