Chemical Composition
0.1
%    
29
%    
59.6
%    (estimate)
1
%    
9.5
%    
0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
600
MPa    
20
% strain    
 
Other Information
Shielded metal-arc welding electrode to weld Mn-steels, tool steels, and for joining stainless steel to dissimilar steels. 113,000 psi TS; 87,000 psi YS; 20% El.
EUTECTRODE E312-16
 