Chemical Composition
0.04 to 0.1
%    
15.5 to 17.5
%    
64.3 to 70.2
%    (estimate)
1.1 to 1.5
%    
0.06 to 0.14
%    
1.2
%  (maximum)  
12.5 to 14.5
%    
0.6 to 0.8
%    
10xC less than or equal to Nb
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
255
MPa    
540 to 740
MPa    
30
% strain    
 