Chemical Composition
0.25 to 0.65
%    
0.05 to 0.1
%    
19 to 22
%    
42.6 to 50.5
%    (estimate)
0.03
%  (maximum)  
30 to 34
%    
0.015
%  (maximum)  
0.25 to 0.65
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
170
MPa    
500 to 750
MPa    
35
% strain    
 