Chemical Composition
0.0015 to 0.005
%    
0.04
%  (maximum)  
16 to 18
%    
65 to 69.9
%    (estimate)
2 to 2.8
%    
0.1 to 0.18
%    
12 to 14
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
260
MPa    
550 to 750
MPa    
35
% strain    
 