Chemical Composition
0.08
%  (maximum)  
16 to 18
%    
62.8 to 70
%    (estimate)
2
%  (maximum)  
2 to 3
%    
12 to 13
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
65
% strain    
 
Other Information