Range attributes
0.15
%  (maximum)  
17 to 19
%    
52
% strain    
67.8 to 74.9
%    (estimate)
2
%  (maximum)  
8 to 10
%    
0.04
%  (maximum)  
0.15
%  (minimum)  
1
%  (maximum)  
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Annealed: At 70 F: 85 ksi TS; 52 El; 66 RA. For high speed automatic machining.
AL TECH TYPE 303EZ
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Annealed: At 70 F: 85 ksi TS; 52 El; 66 RA. For high speed automatic machining.
 
Hyperlink attributes
Integer attributes
ID
60529
231893
 
Further Information



No warranty is given for the accuracy of these data