Range attributes
0.13
%    
15.5
%    
10
% strain    
76.3
%    (estimate)
2.75
%    
1
%    
4.35
%    
1310
MPa    
1140
MPa    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
SCT-heat treatment: 190,000 TS; 165,000 YS; 10 El; 20 RA. For jet engine and missile components; high heat resistance.
AL TECH AM 355
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
SCT-heat treatment: 190,000 TS; 165,000 YS; 10 El; 20 RA. For jet engine and missile components; high heat resistance.
 