Chemical Composition
0.2
%    
25
%    
62.8
%    (estimate)
12
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
331
MPa    
42
% strain    
167
   
 
Other Information