Chemical Composition
0.15
%  (maximum)  
17.5 to 19
%    
70.7 to 74.1
%    (estimate)
0.4 to 0.65
%    
8 to 9.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207 to 276
MPa    
586 to 655
MPa    
55 to 60
% strain    
135 to 145
   
 
Other Information
Heat treated: 85,000-95,000 TS; 30,000-40,000 YS; 55-60 El; 70-75 RA; 135-145 HB; For all welded construction which cannot receive the Strauss heat treatment after welding; radiators, lamps, food and cooking utensils; non-magnetic, austenitic.