Chemical Composition
0.15
%  (maximum)  
23 to 27
%    
43.8 to 57
%    (estimate)
2 to 5
%    
18 to 22
%    
0.03
%  (maximum)  
0.025
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information